Die Zinn-Öllampe weist Schäden aufgrund der Zinnpest auf. Wird Zinn Temperaturen unter 13°C ausgesetzt, beginnt sich seine Struktur umzuwandeln, wodurch das Material unwiederbringlich geschädigt wird. Meistermarke: ICW
The textual information presented here is free for non-commercial usage if the source is named. (Creative Commons Lizenz 3.0, by-nc-sa) Please name as source not only the internet representation but also the name of the museum.Rights for the images are shown below the large images (which are accessible by clicking on the smaller images). If nothing different is mentioned there the same regulation as for textual information applies.Any commercial usage of text or image demands communication with the museum.